Code | Packing |
---|---|
KSS330 | 290 ml Cartridge. |
TECHNICAL DATA
Characteristic | Test Methods | Value |
---|---|---|
Basis | Hybrid MS Polymer | |
Appearance | Paste | |
Curing mechanism | By air humidity | |
Specific Gravity | 1470± 30 kg/m³ | |
Skin formation time | 23°C/50% rel. humid | 15±5min. |
Hardening time | 23°C/50% rel. humid | 2–3mm/day |
Resistance to flow | ISO 7390 | 1–2mm |
Application temperature | between +5°C and +30°C | |
Hardness Shore A | ISO 868 | 45–55 |
Tensile strength (aluminium) | ISO 8339 | 1,7±0,3 MPa |
Tensile strength (glass) | ISO 8339 | 1,7±0,3 MPa |
Module E 100% (aluminium) | ISO 8339 | 1,2±0,3 MPa |
Module E 100% (glass) | ISO 8339 | 1,2±0,3 MPa |
Elongation at break (aluminium) | ISO 8339 | 200±50% |
Elongation at break (glass) | ISO 8339 | 200±50% |
Tensile strength | ISO 37-1 | 2,3±0,3 MPa |
Elongation at break | ISO 37-1 | 250±50% |
Temperature resistance | between -40°C to +90°C |